BiFeO3 (BFO) has been shown to have great potential for many applications due to a number of attractive properties, such as its multiferroic nature at room temperature, high Curie temperature (TC ~ 830 oC), and high remanent polarization. Thus, various piezoelectric devices, for example, sensors, actuators and transducers, can be prepared using an active layer of BFO-based materials integrated onto substrates as thick films. But, the processing of the BFO thick films is challenging due to readily occurring chemical reactions between the substrate, electrode and BFO layer. The present literature data does not provide the necessary information on the preparation conditions that could be used to improve the quality of BFO thick films on a broader basis.
The purpose of this PhD thesis was to study the interactions between different substrates and the BFO films and thus be able to prepare high-quality BFO thick films in terms of phase composition and microstructure.
In the first part of this dissertation we provide a comprehensive investigation of BFO thick films prepared by screen-printing and their interactions with ceramic (Au/Al2O3) and metal (Ag, Au, Pt) substrate materials during processing. We show that the microstructure and phase composition of the BFO thick films is strongly dependent on two parameters, i.e., the impurity present in the electrode and the sintering temperature. By optimizing the sintering temperature (740 oC), and by using a high-purity Ag metal substrate we successfully prepared dense and nearly single-phase BFO thick films. While the local ferroelectric behavior of this film has been confirmed by piezo-response force microscopy analysis, its macroscopic electrical response is characterized by a high electrical conductivity coupled with an interface-related, diode-like, current-voltage behavior.
However, not only is it challenging to prepare high-quality BFO thick films due to processing issues, but it is problematic to pole the material due to its high coercive field and high electrical conductivity. The results of the last part of the dissertation suggest an alternative way of poling BFO films by sintering (annealing) at a temperature above the ferroelectric-paraelectric phase transition, overcoming the obstacle of poling the BFO “ex-situ” using large external electric fields. Direct and converse piezoelectric measurements confirmed that the as-sintered BFO thick films on Pt/Al2O3 substrates yield d33 values of up to ~20 pC/N. It was observed that a significant self-poling effect only appears in cases when the films are heated and cooled through the TC (~ 820 oC). These self-poled films exhibit a microstructure with randomly oriented columnar grains. The compressive strain gradient across the film thickness cooled from above the TC was experimentally confirmed and is suggested to be responsible for the self-poling effect.