Views: 0 | Downloads: 0
The barium strontium titanate solid solution, BaxSr1-xTiO3, is a ferroelectric material suitable for applications in microwave-tunable devices. Its Curie temperature strongly depends on the Ba/Sr ratio, and the compositions that are in the paraelectric phase in the operating temperature range, yet still close to the phase-transition temperature, exhibit high permittivity, high tunability and at the same time also low dielectric losses in the microwave frequency range. But to achieve the above requirements with solution-derived thin films different processing-related film characteristics, i.e., the film thickness, microstructure (grain size and shape, porosity), residual stress, etc., should be considered since they strongly influence the functional response of the films.
The Ba0.5Sr0.5TiO3 (BST 50/50) films with thicknesses in the range from 90 nm to 600 nm were prepared on polycrystalline alumina substrates by repeating the deposition of a hetero-metallic precursor solution by spin-coating, drying, pyrolysis, and rapid thermal annealing steps (multi-step annealing) at 900 °C until the required film thickness has been reached. The microstructure of the films is dense and predominantly columnar. The room-temperature dielectric properties in the kHz and GHz frequency ranges show a non-monotonic film-thickness dependence, which can be divided into three groups. Firstly, for the thicknesses between 90 nm and 170 nm, the dielectric permittivity of the films is controlled by the dielectric grain-size effect; it increases from 650 to 1250 measured at 100 kHz as the grain size increases from ~45 nm to ~80 nm for the 90-nm- and 170-nm-thick films, respectively. For these films a high biaxial tensile stress of ~350 MPa is observed and related to the thermal-expansion mismatch between the film and the substrate. For the film thicknesses between 170 nm and 240 nm, the dielectric permittivity reaches plateau values between 1250 and 1350, corresponding to only a slight change of the grain size from ~80 nm to ~90 nm. In parallel, the tensile stress decreases to 198 MPa. But in the third thickness range the permittivity drops to 770 for the 600-nm-thick film, while the grain size changes only slightly. We ascribe this drop of the permittivity to the existence of intergranular cracks that form as a consequence of the relaxation of the tensile residual stress, which can be explained by the brick-wall model.
In the second part we focus on a study of the crystallization and evolution of the microstructure of BST 50/50 thin films prepared by multi-step annealing at temperatures between 600 °C and 900 °C. The films, consisting of seven layers deposited from the precursor solution, crystallize in a pure perovskite phase after annealing at ~640 °C and have a granular microstructure. The latter forms upon the annealing of individual deposited layers with the individual layer thickness much larger than the grain size, and persists upon annealing up to ~800 °C. Upon annealing at high enough temperatures (≥880 °C) the grain size exceeds the individual layer thickness, resulting in a predominantly columnar microstructure upon repeating the deposition-drying-pyrolysis-annealing steps. The evolution of such a columnar microstructure proceeds via the crystallization and growth of fine, equiaxed grains of 10–20-nm across within an individual, ~40-nm-thick layer on top of pre-existing columnar grains followed by homo-epitaxial overgrowth within each grain.